Weld Quality Evaluation Method for the Resistance Spot Welds using X-ray Transmission Inspection
Jong-Dae Lee, So-Jeong Lee, Jung-Hwan Bang, Gil-Sang Yoon, Mok-Soon Kim, Jun-Ki Kim
J Weld Join. 2014;32(6):537-543.   Published online December 31, 2014
PDFPDF    
2031586
Resistance Spot Welding Characteristics of Mg Alloy Applying Current Waveform Control
Dong-Soon Choi, In-Sung Hwang, Dong-Cheol Kim, Jae-Wook Ryu, Moon-Jin Kang
J Weld Join. 2014;32(2):196-201.   Published online May 14, 2014
PDFPDF    
2031545
Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode
Dong-Soon Choi, In-Sung Hwan, Dong-Cheol Kim, Moon-Jin Kang
J Weld Join. 2013;31(6):27-31.   Published online January 21, 2014
PDFPDF    
2031510
Resistance Spot Welding Characteristics of Mg Alloy Using Process Tape
Dong-Soon Choi, Dong-Cheol Kim, Moon-Jin Kang
J Weld Join. 2013;31(3):49-53.   Published online June 30, 2013
PDFPDF    
Analysis of Microstructure for Resistance Spot Welded TRIP Steels using Atomic Force Microscope
Chul Young Choi, ChangWook Ji, Dae-Geun Nam, Jaeho Jang, Soon Kook Kim, Yeong-Do Park
J Weld Join. 2013;31(1):43-50.   Published online June 5, 2013
A Study on the Arc Position which Influence on Quality of Plug Welding in the Vehicle Body
Kyungmin Lee, Jaeseong Kim, Boyoung Lee
J Weld Join. 2012;30(3):66-70.   Published online July 18, 2012
PDFPDF    
Hardness Distribution and Microstructures of Electric Resistance Spot Welded 1GPa Grade Dual Phase Steel
Hye-Sung Na, Jong-Pan Kong, Tae-Kyo Han, Kwang-Geun Chin, Chung-Yun Kang
J Weld Join. 2012;30(2):76-80.   Published online May 16, 2012
PDFPDF    
Influence of Welding Parameters on Macrostructure and Mechanical Properties of Friction-Stir-Spot-Welded 5454-O Aluminum Alloy Sheets
Won-Ho Choi, Yong-Jai Kwon, Sung-Ook Yoon et al.
J Weld Join. 2011;29(6):56-64.   Published online January 20, 2012
PDFPDF    
Effect of Si content on Nugget Diameter of Electric Resistance Spot Welded Dual Phase Steel
Jong-Pan Kong, GilMo Kang, Tae-Kyo Han, Kwang-Geun Chin, Chung-Yun Kang
J Weld Join. 2011;29(5):99-105.   Published online November 22, 2011
PDFPDF    
A Study on the Crash Characteristics and Analysis of Spot+adhesive Welds in Automobile B-pillar Parts
Youngsoo Choi, Sangman Yun, Yongjoon Cho, Se-hun Rhee
J Weld Join. 2011;29(5):72-81.   Published online November 22, 2011
PDFPDF    
A Study on Anti-Oxidation of Stainless Steel Spot Weld
DongWoon Huh, Sehun Rhee
J Weld Join. 2011;29(5):58-62.   Published online November 22, 2011
PDFPDF    
Dynamic Model for Electrode Expansion in Resistance Spot Welding Machines
SyedAsadUllah Shah, HeeSeok Chang
J Weld Join. 2011;29(2):94-101.   Published online May 7, 2011
PDFPDF    
Effects of Tool Speed on Joining Characteristics during Friction Stir Spot Welding of Mg-alloy(AZ31B) Sheet
Hyung-Seop Shin, Yoon-Chul Jung, Kwang Choi
J Weld Join. 2011;29(2):80-87.   Published online May 7, 2011
PDFPDF    
In-Process Monitoring of Micro Resistance Spot Weld Quality using Accelerometer
HeeSeok Chang, HyoChul Kwon
J Weld Join. 2011;29(1):115-122.   Published online March 4, 2011
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI